Material Notes:
The VICOTE F808 natural, F809 natural and F810Blk grades have been specifically formulated to provide a resilient coating with high wear and abrasion resistance combined with excellent release properties on ferrous substrates such as carbon and cast steels. These properties are retained at high temperatures where other release coatings would potentially fail. VICOTE dispersions have a low level of extractables.All information provided by Victrex.
Physical Properties Metric English Comments
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 1kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.104
0.104
µm @ 10 min., Using 250N Load; ASTM G 133
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Konig Hardness (seconds) 170
ISO 1522
Users viewing this material also viewed the following: