Material Notes:
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.Information provided by Washington Penn Plastic Co.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.27 MPa
3375 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Elongation at Yield 8.5 %
8.5 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
1% Secant; ASTM D790
1.97 GPa
285 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Gardner Impact 7.23 J

@Temperature -30.0 °C
5.33 ft-lb

@Temperature -22.0 °F
ASTM D5420
18.1 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648