Weartech International WT-C Nickel Hardfacing & Wear Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Weartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Weartech International WT-C Nickel Hardfacing & Wear Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: seals, sleeves and dies, plastic extrusion, agitator bearings, pump impellers, ball valvesInformation provided by Weartech International
Mechanical Properties Metric English Comments
Hardness, Rockwell C 20 - 26
20 - 26
Hardness, Vickers 150

@Treatment Temp. 760 °C
150

@Treatment Temp. 1400 °F
180

@Treatment Temp. 649 °C
180

@Treatment Temp. 1200 °F
185

@Treatment Temp. 538 °C
185

@Treatment Temp. 1000 °F
190

@Treatment Temp. 25.0 °C
190

@Treatment Temp. 77.0 °F
190

@Treatment Temp. 427 °C
190

@Treatment Temp. 800 °F
Component Elements Properties Metric English Comments
Carbon, C 0.12 %
0.12 %
Chromium, Cr 16 %
16 %
Iron, Fe 5.5 %
5.5 %
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo 17 %
17 %
Nickel, Ni 59.48 %
59.48 %
Silicon, Si 0.80 %
0.80 %
Vanadium, V 0.30 %
0.30 %