Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF1811-BK1 15% Glass Fiber Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183-87
Filler Content 15 %
15 %
Linear Mold Shrinkage, Flow 0.0065 - 0.0105 cm/cm
0.0065 - 0.0105 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0095 - 0.0135 cm/cm
0.0095 - 0.0135 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 165 MPa
23900 psi
ISO 178-93
Flexural Modulus 5.40 GPa
783 ksi
ISO 178-93
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ISO 75-93