Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 180 MPa
26100 psi
ISO 178-93
Flexural Modulus 7.50 GPa
1090 ksi
ISO 178-93
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75-93