Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | |
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | DIN 53461 |
Qualchem Danamid AFGFH-30 Polyamide 66, 30% Glass Fiber Reinforced with glass fiber. Heat stabilized, for long-lasting use at 120-140°C.Information provided by Qualchem Zrt. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 3.18 mm |
446 °F @Thickness 0.125 in |
Unannealed; ISO 75-2/A |
PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ASTM D648 |
Kolon KOPA® KN333MT30BL Mineral Reinforced Nylon 66 MF reinforcedApplications Cam shaftsInformation provided by API-Kolon. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | |
LATI Latamid 66 MDT03-01 PA 66 Polyamide 66 (PA66) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem AUT230M PEI Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem AUT230M PEI (Europe-Africa-Middle East) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 6.40 mm |
446 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ISO 75-93 |
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Developmental Grade Nylon 66 Description: Mineral/Glass Reinforced Developmental Grade Nylon 66Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | GB1634 |
Zhejiang Juner PA-A6-66H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide Applications: Cover of Mini MCBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ASTM D648 |
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ISO 75 |
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 230 °C | >= 446 °F | |
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-60 PA666-GF60 Product description: Grilon TSG-60 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers. Grilon TSG-60 has the following important properties: Very high st.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ASTM D648 |
DuPont Performance Polymers VESPEL TP-8395 Polyimide DuPont Vespel TP-8395 parts are specified for high-temperature and high-wear applications. TP-8395 parts offer an excellent balance of mechanical and thermal properties for superior performance in a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ASTM D648 |
Beijing Chemical Industry KAIFA® 3030F PET Resin High mechanical strength, Creep resistant, Low friction, High crystallizationInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | ISO 75-2/AF |
Addiplast Addinyl C2 V20 Nylon 66/6, 20% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Valox® V9230CS PET (Europe-Africa-Middle East) 15% GF PET Injection Moulding grade, Heat and Color Stabilised, for light colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C | 446 °F | |
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |