Material Notes:
Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available in ribbon form in a variety of widths and thickness. Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 16.0 g/cc
0.578 lb/in³
Component Elements Properties Metric English Comments
Gold, Au 69 %
69 %
Platinum, Pt 6.0 %
6.0 %
Silver, Ag 25 %
25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000158 ohm-cm
0.0000158 ohm-cm
Descriptive Properties Value Comments
ASTM Equiv. B552
Compare To: WE 1
Tempers Available AR,A