All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 11.2 g/cc
0.405 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 23.4 MPa
3400 psi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 26.0 W/m-K
180 BTU-in/hr-ft²-°F
Melting Point 299 - 304 °C
570 - 579 °F
Solidus 299 °C
570 °F
Liquidus 304 °C
579 °F
Component Elements Properties Metric English Comments
Lead, Pb 95.5 %
95.5 %
Silver, Ag 2.5 %
2.5 %
Tin, Sn 2.0 %
2.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00002263 ohm-cm
0.00002263 ohm-cm