Wingate Alloys Winco HCP Hard Chromium Plated Turned, Ground and Polished Shafting

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Wingate Alloys
Trade Name Winco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wingate Alloys Winco HCP Hard Chromium Plated Turned, Ground and Polished Shafting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A corrosive resistant shafting for piston rod and hydraulic piston applications.Winco HCP introduces a new concept in turned, ground and polished, hard chromium plated bars. The hardness, toughness and close tolerances are combined with the chromium plating to supply the corrosion resistance necessary for all Rod applications.Advantages:Supplied in finished product form or can be machined with ordinary high speed tools.Protected by new process that seals in microscopic cracks that may occur in the hard chroming procedure.More than doubles corrosive resistance of standard chrome plated bars.Turned to extremely close tolerances and then hard chrome plated. Applications: Shafting – all types, equipment pistons, hydraulic piston rods, dowel pins, guide pins and pneumatic piston rodsInformation from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 65
65
Case
Tensile Strength, Yield >= 862 MPa
>= 125000 psi
Descriptive Properties Value Comments
Depth of Plating (in) 0.001
Micro Finish of Case (RMS) 8