Wingate Alloys Winco NS Non-Skid Safety Material

Category Metal
Manufacturer Wingate Alloys
Trade Name Winco
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wingate Alloys Winco NS Non-Skid Safety Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
To eliminate hazardous and slippery environments.Winco NS exceeds OSHA and UL standards for safety and slip resistance and outlasts all competitive materials. Advantages:Available: Carbon Steel, Aluminum and Stainless Steel.Plate or Grating: Provided in standard industry sizes.Surface Roughness and Finishes: Choice of fine, medium or coarse.Workability: Can be welded, flame-cut, sheared, drilled and punched through surface.Cleans: Easily by all standard industrial cleaning methods.Wearability: Alloy forms a long lasting, file hard, martensitic surface. Applications: Floors, ramps, stairs, machine platforms, catwalks, wet decks, trench grating, stair treads and nosings.Information from Wingate Alloys Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62
62