Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeus THV Tubing

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Zeus
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeus THV Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.
Physical Properties Metric English Comments
Density 1.95 - 2.06 g/cc
0.0704 - 0.0744 lb/in³
ASTM D792
Water Absorption <= 0.030 %
<= 0.030 %
ASTM D257
Crystallinity 26 - 29 %
26 - 29 %
Mechanical Properties Metric English Comments
Hardness, Shore D 44 - 58
44 - 58
ASTM D2240
Tensile Strength, Ultimate 20.0 - 29.0 MPa
2900 - 4210 psi
ASTM D638
Elongation at Break 420 - 600 %
420 - 600 %
ASTM D638
Modulus of Elasticity 0.240 GPa
34.8 ksi
ASTM D638
Flexural Modulus 0.320 - 0.520 GPa
46.4 - 75.4 ksi
ASTM D790
Coefficient of Friction 0.80
0.80
Thermal Properties Metric English Comments
Melting Point 120 - 185 °C
248 - 365 °F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Glass Transition Temp, Tg 5.00 - 36.0 °C
41.0 - 96.8 °F
Decomposition Temperature 420 - 440 °C
788 - 824 °F
ASTM E1131
Oxygen Index 65 - 75 %
65 - 75 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.3502
1.3502
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 2.4 - 6.6

@Frequency 1.00e+6 Hz
2.4 - 6.6

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 48.0 - 61.8 kV/mm
1220 - 1570 kV/in
ASTM D149
Descriptive Properties Value Comments
Radiation Resistance (MRad) 20