Thermal Properties Metric English Comments
Decomposition Temperature 420 - 440 °C
788 - 824 °F
ASTM E1131
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.