ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers and high purity inorganic binders. It offers low thermal conductivity, excellent thermal shock resistance and is an effective thermal insulator in numerous thermal process systems. It is also well-suited for applications experiencing vibration, mechanical stress and strong erosive forces. The excellent rigidity and modulus of rupture possessed by this board makes it strong and self-supporting, yet relatively lightweight and easy to cut or machine. This product's features allow for quick, efficient handling and high installation rates, thereby enabling fast turnaround times in a variety of industrial insulation applications. Once installed, it can help reduce energy costs and cycling times due to its high insulating capability, as well as serving to protect refractory surfaces from thermal shock. Type RSBD-HD Board exhibits excellent chemical stability, resisting attack by most corrosive agents. Exceptions are hydrofluoric, phosphoric, hydrochloric and sulfuric acids as well as concentrated alkalis. It will also resist oxidation and reduction to a certain point. If wet by water, steam or oil upon drying all properties will be restored.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 0.419 g/cc
0.0151 lb/in³
Loss On Ignition 6.0 - 7.0 %
6.0 - 7.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00210 GPa
0.305 ksi
parallel to thickness
0.000870 GPa

@Temperature 1010 °C,
Time 86400 sec
0.126 ksi

@Temperature 1850 °F,
Time 24.0 hour
parallel to thickness
Compressive Yield Strength 0.240 MPa
34.8 psi
at 5% compression ,after 24 hrs at 1010°C, parallel to thickness
0.400 MPa
58.0 psi
at 5% compression, parallel to thickness
Thermal Properties Metric English Comments
Thermal Conductivity 0.110 W/m-K

@Temperature 204 °C
0.763 BTU-in/hr-ft²-°F

@Temperature 399 °F
0.170 W/m-K

@Temperature 649 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 1200 °F
0.220 W/m-K

@Temperature 1010 °C
1.53 BTU-in/hr-ft²-°F

@Temperature 1850 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Shrinkage <= 5.00 %

@Temperature 1200 °C,
Time 14400 sec
<= 5.00 %

@Temperature 2190 °F,
Time 4.00 hour
Component Elements Properties Metric English Comments
Al2O3 60 - 65 %
60 - 65 %
SiO2 10 - 15 %
10 - 15 %
Electrical Properties Metric English Comments
Dielectric Strength 1.06 kV/mm
27.0 kV/in
Descriptive Properties Value Comments
Color White
Kaolin Clay, % 15 to 20
Organic Content, % 5 to 10