Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.170 W/m-K @Temperature 815 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 260 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 200 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler BF-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 400 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group V-1100 410 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 649 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 980 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1800 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 1100 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 1100 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 2010 °F |
parallel to thickness |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 538 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 260 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials BNZ-23HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 400 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 427 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 801 °F |
|
BNZ Materials Marinite® P High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |