Zotefoams Plastazote® LD45IC Low Density Polyethylene Foam, Intermediate Cell

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Zotefoams
Trade Name Plastazote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams Plastazote® LD45IC Low Density Polyethylene Foam, Intermediate Cell.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0370 - 0.0470 g/cc
0.00134 - 0.00170 lb/in³
sheet density
Cell Length 0.500 - 1.00 mm
0.0197 - 0.0394 in