Polyethylene Terephthalate (PET)
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Category :
Polyethylene Terephthalate (PET), 20% Glass Reinforced
Product List
Manufacturer
A. Schulman, Inc.
-
Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
DSM Engineering Plastics
DuPont Performance Polymers
Eurotec
Kingfa Sci. & Tech. Co.
Kolon
Lavergne Performance Compounds
Polyram
Shinkong Synthetic Fibers Corp
Tisan Engineering Plastics
Tips:
Max 50 items displayed. For more, contact customer service.
PRODUCT NO.
Manufacturer
Trade Name
DuPont Performance Polymers Rynite® 415HP BK503 PET (Unverified Data**)
DuPont Performance Polymers Rynite® FR515 BK507 PET (Unverified Data**)
DuPont Performance Polymers Rynite® GW520CS NC010 PET (Unverified Data**)
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled (discontinued **)
Custom Resins Vexel™ E20GF15 , 15% Glass Reinforced PET (discontinued **)
Polyram PE322G22 PET, 22% Glass Fiber (discontinued **)
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET)
Kolon
KOPET®
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant
Lavergne Performance Compounds
VYPET
Lavergne VYPET VNT 615 HP PET 15% Glass Reinforced
Lavergne Performance Compounds
VYPET
Kingfa PET-G15 15% Glass Fiber Reinforced PET
Kingfa Sci. & Tech. Co.
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Lavergne Performance Compounds
VYPET
Techmer ES HiFill FR® PET GF15 FR 15% Glass Filled
Techmer ES
HiFill FR®
Techmer ES HiFill® PET GF15 IM 15% Glass Filled
Techmer ES
HiFill®
Techmer ES HiFill® PET GF15 X BK 15% Glass Filled
Techmer ES
HiFill®
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled
Techmer ES
HiFill®
Shinkong Synthetic Fibers Shinite® T102G15 PET, 15% Glass Filled, Fire Retardant
Shinkong Synthetic Fibers Corp
Shinite®
Techmer ES HiFill FR® PET GF15 IM FR X 15% Glass Filled
Techmer ES
HiFill FR®
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
A. Schulman, Inc.
SCHULADUR®
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate
Tisan Engineering Plastics
TISAPET®
Polyram RamSter PE304G3 PET, 15% Glass Fiber
Polyram
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
DSM Arnite® AV2 340 PET-20% Glass Reinforced (European Grade)
DSM Engineering Plastics
Arnite®
DuPont Performance Polymers Rynite® 415HP BK503 Polyethylene Terephthalate (PET) (Unverified Data**)
DuPont Performance Polymers
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET) (Unverified Data**)
DuPont Performance Polymers
DuPont Performance Polymers Rynite® 515CS BK575M PET
DuPont Performance Polymers
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Eurotec
Tecopet®
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Eurotec
Tecopet®
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Eurotec
Tecopet®
Eurotec® Tecopet® PT70 GR15 NL100 MB PET, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Eurotec
Tecopet®
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Eurotec
Tecopet®
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Eurotec
Tecopet®
BASF Petra® 110 BK-112 15% Glass Filled PET
BASF
Petra®
BASF Petra® 7010 BK 5830 15% Glass Filled PET
BASF
Petra®
BASF Petra® 7010 WT 7729 15% Glass Filled PET
BASF
Petra®
Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber
Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Cheng Yu Plastic E2315 Flame Retardant PET, 15% Glass Fiber
Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
DuPont Performance Polymers Rynite® 415HP NC010 PET (Unverified Data**)