Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 20% Glass Reinforced
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Linear Mold Shrinkage 0.0025 - 0.011 cm/cm
0.0025 - 0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 120
120
ASTM D785
Tensile Strength, Yield 1.24 MPa
179 psi
ASTM D638
Flexural Yield Strength 178 MPa
25900 psi
ASTM D790
Izod Impact, Notched 0.863 J/cm
1.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Flammability, UL94 V-0
V-0