| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 Amber 9360 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 Amber 9375 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 Clear 9460 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 CLR 9500 Polyvinyl Chloride, Rigid (PVC, Rigid)
The formula has a green blue tintInformation provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 Polyvinyl Chloride, Rigid (PVC, Rigid)
This product is available in opaque and transparent colors.Information provided by PolyOne
|
|||
| Density | <= 0.833 g/cc | <= 0.0301 lb/in³ | ASTM D1505 |
|
PolyOne Geon™ Vinyl Packaging 2710 TRN 9470 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | |
|
Pyrotek Pyroboard™ S1000 Roller
Pyroboard™ S1000 is designed to be used throughout the preheat and cooling sections of the furnace.Information provided by Pyrotek.
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | |
|
Pyrotek Pyroboard™ S1300 Roller
Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.Information provided by Pyrotek.
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® DX231 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene
This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c..
|
|||
| Density | 0.833 - 0.837 g/cc | 0.0301 - 0.0302 lb/in³ | BRCP 4843 |
|
ExxonMobil EXXAL® 9 Isononyl Alcohol
CAS Number: 68526-84-1Information provided by ExxonMobil
|
|||
| Density |
0.833
g/cc <br>@Temperature 15.6 °C
|
0.0301
lb/in³ <br>@Temperature 60.1 °F
|
ASTM D4052 |
|
ExxonMobil SpectraSyn™ 8 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) ..
|
|||
| Density | 0.833 - 0.834 g/cc | 0.0301 - 0.0301 lb/in³ | |
|
BASF 2-Ethylhexanol
Formula: C8H18OCAS: 104-76-7Description: 2-Ethylhexanol is a clear, colorless, mobile and neutral liquid with a characteristic odor. It is miscible with most common organic solvents, but its miscibi..
|
|||
| Density | 0.833 - 0.913 g/cc | 0.0301 - 0.0330 lb/in³ | Average value: 0.847 g/cc Grade Count:12 |
|
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Mitsui TPX® DX820 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
|
|||
| Density | 0.834 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
|
|||
| Density | 0.833 g/cc | 0.0301 lb/in³ | ASTM D1505 |
|
Mitsui TPX® RT18 XB Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
|
|||