Polymer Property : Density = 0.0426 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate
Information provided by Ravago
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Density 1.18 g/cc
0.0426 lb/in³
ISO 2781
Huntsman AVALON® 65 AB Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
Density 1.18 g/cc
0.0426 lb/in³
ISO 2781
Lubrizol Advanced Materials Pearlstick® D40-70/33 Linear Thermoplastic Polyurethane
Pearlstick D40-70/33 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. S..
Density 1.18 g/cc
0.0426 lb/in³
Momentive Performance Materials RTV8111 White General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183/A
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5..
Density 1.18 g/cc
0.0426 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific)
LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P..
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Density 1.18 g/cc
0.0426 lb/in³
JIS K-6911
Unitika elitel UE3220 Polyester, Flake
Adhesive agent, Resin modifier, Soft type, Standard resinUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a..
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Wanhua Chemical Wanthane® WHT-1180 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183-87
Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6
Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman.
Density 1.18 g/cc
0.0426 lb/in³
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix
HexPly® M49 is a 120°C curing toughened epoxy matrix with good impact resistance suitable for use in performance cars. The matrix is highly tolerant of a wide variety of production techniques and ..
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009...
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l..
Density 1.18 g/cc
0.0426 lb/in³
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat..
Density 1.18 g/cc
0.0426 lb/in³
(DAM); ISO 1183
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO R 1183
Fainplast Compounds GS 63 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO R 1184
Fainplast Compounds MPH 69/D Medical Flexible PVC, Extrusion
Technical tubes no DOP
Density 1.18 g/cc
0.0426 lb/in³
Arlon SQA-TMS-024
Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: MylarAppearance: Pink high viscosity gumThis data represents typical values for the production material. The data..
Density 1.18 - 1.22 g/cc
0.0426 - 0.0441 lb/in³
ISO 1183
Austin Novel Materials Texalan® 282A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Density 1.18 g/cc
<br>@Temperature 23.0 °C
0.0426 lb/in³
<br>@Temperature 73.4 °F
ISO 1183
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Density 1.18 g/cc
0.0426 lb/in³
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, General Description &nbsp;(discontin
Product form is white, odorless chips. Distinguishing Feature: Low viscosity polymer. Improves processing of dry stiff stocks.35 % Chlorine Content. 1% Sulfur Content. Excellent Abrasion Resista..
Density 1.18 g/cc
0.0426 lb/in³
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend &nbsp;(discontinued **)
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin..