Polymer Property : Density = 0.0455 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
DIN 53479
Qualchem Danamid FELX0 Polyamide 6
Flame retardant, halogen-free (V-0)Information provided by Qualchem Zrt.
Density 1.26 g/cc
0.0455 lb/in³
ASTM D1475
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive  (discontinued **)
CX-943 is a one-component polyurethane-based squeegee-grade, structural adhesive. Its elastomeric properties enable it to move with substrates as it expands and contracts. The patented formula is ..
Density 1.26 g/cc
0.0455 lb/in³
Dry As Molded
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH  (dis
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre..
Density 1.26 g/cc
0.0455 lb/in³
Amorphous; ISO 1183
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.26 g/cc
0.0455 lb/in³
Eastman Tenite 105-33 Cellulose Acetate  (discontinued **)
33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Density 1.26 - 1.29 g/cc
0.0455 - 0.0466 lb/in³
309-1D Resin
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive
Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh..
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC
LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Techmer ES HiFill® PA12 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Density 1.26 g/cc
0.0455 lb/in³
JIS K-6911
Unitika elitel UE3300 Polyester, Flake
Low molecular weight type UE3210, High OH type, Branched & highly crosslinkedUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro..
Density 1.26 g/cc
0.0455 lb/in³
Cured resin density
Hexcel® HexPly® 108 180°C Curing Epoxy Matrix
HexPly® 108 is a high temperature resistant epoxy resin system developed for the fabrication of primary aircraft and space structures. 108 has excellent hot wet properties and exhibits low viscosit..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
DSM Arnitel® PL650 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds FR 008 Flexible PVC, Insulation
Insulation
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds PK 0111 Flexible PVC, Lead Free
Gas pipe according to DIN 4815
Density 1.26 g/cc
0.0455 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr..
Density 1.26 g/cc
0.0455 lb/in³
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.26 g/cc
0.0455 lb/in³
A. Schulman ComAlloy Hiloy® 249 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
DSM Arnitel® PM650 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds PHS 80/B Flexible PVC, Transparent Extrusion
Pipes low migration
Density 1.26 - 1.65 g/cc
0.0455 - 0.0596 lb/in³
Average value: 1.48 g/cc Grade Count:12
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Eurostar Star L PA66 15Y D61 PA66, Carbon Filled, Injection Molded
Star L PA66 15Y D61 is a PTFE/Silicone Oil Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.