Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.05 - 2.15 g/cc | 0.0741 - 0.0777 lb/in³ | ASTM D792 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Density | 2.05 - 2.15 g/cc | 0.0741 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.00 - 2.15 g/cc | 0.0723 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.95 - 2.15 g/cc | 0.0704 - 0.0777 lb/in³ | |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.10 - 2.15 g/cc | 0.0759 - 0.0777 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss.. |