| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO)
PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of ..
|
|||
| Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
|
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | DIN 53479; ASTM D792 |
|
Kolon KOPA® KN173HI3R High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® B 238 Black 21 N PA66/6, Conditioned
Description: Unreinforced and modified copolyamide 66/6, heat stabilized, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 238 is particular..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12
LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D 792 |
|
Shakespeare Isocorâ„¢ TT52SI Nylon 6 Terpolymer
Isocorâ„¢ TT52SI multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ TT52SI is easily processed and has a wide range of application..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12
LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Solvay GERONOL® PSI Surfactant
Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Soluble in water and most polar and aromatic solventsAvailable in: Asia Pacific, Europe, Latin Am..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Solvay GEROPON® DOS/PG Surfactant
Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN GLYCOL WATER SOLUTIONCAS: 577 – 11 – 7; 57 – 55 – 6; 7732 – 18 – 5Solubility: Dispersible in water and polar solvents. ..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Solvay SOPROPHOR® 796/P Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOPROPOXYLATED POLYARYLPHENOLCAS: 70880 – 56 – 7Solubility: Soluble in water and most polar and aromatic sol..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Plastics Group Polifil® 625L Nylon 6/6 (DAM)
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group...
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Chase Plastics CP Pryme® NN100TL (Dry) Nylon 66, Lubricated, Impact Modified
Features: LubricatedImpact modifiedGood toughnessForm: PelletsInformation provided by Chase Plastics.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Loctite® 493 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Loctite® 675 Medium Strength Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
Eurostar Starpylen MX05038 TPEX, Injection Molded
Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
Eurostar Staramide Z1000XXC PA66, Injection Molded
Staramide Z1000XXC is an UV Stabilized Polyamide 66 Injection Molding Resin (also known as R1000HI0944)Information provided by Eurostar.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
Eurotec® Tecolen® CP20 MF20 NL XC30 PPCP, 20% mineral filled, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183 |
|
Eurotec® Tecomid® NB50 NL IT PA 6 super tough
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | |
|
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry)
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good ..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon UltraPad™ 55073R031 Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ISO 1183/A |
|
Addiplast Addinyl C2 R Nylon 66/6
High impact resistanceInformation provided by Addiplast.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Ashley Polymers Ashlene® 736LD Nylon 6
Modified to retain toughness at low temperatures for injection molding.Data provided by the manufacturer
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | AboCast 7802-1 |
|
Abatron AboCast 7802-1/AboCure 50-12 Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101..
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | ASTM D792 |
|
Techmer ES Luriblend® ABS TL10
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Density | 1.09 g/cc | 0.0394 lb/in³ | Latex |
|
DuPont Performance Polymers AquaStik® AQS-1120 Polychloroprene Latex
(discontinued **)
Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features mechanical stabil..
|
|||