| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | packed |
|
Imerys Minsparâ„¢ 4 Ground Feldspar
Minsparâ„¢ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excel..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Loose |
|
Excalibar ExBar™ W 2 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Loose |
|
Excalibar ExCal® 200 Calcium Carbonate CaCO3 Powder
ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Tapped |
|
CIMBAR Gel Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | Tapped |
|
CIMBAR RP 9305 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
CIMBAR Suspengel™ 325 High Purity Bentonite, Industrial Grade
Suspengel products are manufactured from the highest quality Western Bentonite reserves. Suspengel products are easy to disperse thixotropes with excellent suspension properties. Strict process co..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® EXAD 3000 Polyvinylidene Fluoride - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Extrusion aid, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanic..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Bulk Density | 0.961 g/cc | 0.0347 lb/in³ | |
|
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||