Polymer Property : Fiber Count = 1200 denier Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Fiber Count 1330 - 1470 dtex
1200 - 1320 denier
Voloknohim Filament Nylon Linear Density 140 tex
Application: for production of goods for fishery and for other technical purposes. The produced yarn is bright, UV-stabilized, thermostabilized, UV-thermostabilized, not dyed, dyedInformation provi..
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-11 Industrial Woven Fabric 312
Information provided by 3M
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
Fiber Count 1330 dtex
1200 denier
roving
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M