Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0125 cm/cm Grade Count:219 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | Average value: 0.00144 cm/cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00289 cm/cm Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00250 cm/cm Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00256 cm/cm Grade Count:72 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00700 cm/cm Grade Count:14 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00669 cm/cm Grade Count:113 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.0133 cm/cm Grade Count:60 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0300 cm/cm Grade Count:123 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00214 cm/cm Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00743 cm/cm Grade Count:56 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00226 cm/cm Grade Count:36 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00631 cm/cm Grade Count:12 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0280 cm/cm | 0.00100 - 0.0280 in/in | Average value: 0.0135 cm/cm Grade Count:111 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.0118 cm/cm Grade Count:49 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0150 cm/cm | 0.00100 - 0.0150 in/in | Average value: 0.00430 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0120 cm/cm | 0.00100 - 0.0120 in/in | Average value: 0.00366 cm/cm Grade Count:16 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00550 cm/cm | 0.00100 - 0.00550 in/in | Average value: 0.00139 cm/cm Grade Count:21 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00525 cm/cm Grade Count:7 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0500 cm/cm | 0.00100 - 0.0500 in/in | Average value: 0.00570 cm/cm Grade Count:30 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00429 cm/cm Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00455 cm/cm Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0226 cm/cm | 0.00100 - 0.0226 in/in | Average value: 0.00526 cm/cm Grade Count:33 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00240 cm/cm Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0250 cm/cm | 0.00100 - 0.0250 in/in | Average value: 0.0122 cm/cm Grade Count:14 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00356 cm/cm Grade Count:16 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0170 cm/cm | 0.00100 - 0.0170 in/in | Average value: 0.00851 cm/cm Grade Count:16 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |