| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Overview of materials for Silicone Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.700 - 3.80 g/cc | 0.0253 - 0.137 lb/in³ | Average value: 1.31 g/cc Grade Count:923 |
| Water Absorption | 0.0300 - 3.00 % | 0.0300 - 3.00 % | Average value: 1.57 % Grade Count:48 |
| Viscosity | 1.00 - 610000 cP | 1.00 - 610000 cP | Average value: 46500 cP Grade Count:86 |
| Thickness | 12.7 - 52400 microns | 0.500 - 2060 mil | Average value: 551 microns Grade Count:631 |
| Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0300 cm/cm Grade Count:123 |
| Outgassing - Total Mass Loss | 0.100 - 1.07 % | 0.100 - 1.07 % | Average value: 0.584 % Grade Count:7 |
| 0.100 - 0.340 % <br>@Temperature 218 - 218 °C |
0.100 - 0.340 % <br>@Temperature 425 - 425 °F |
Average value: 0.220 % Grade Count:1 | |
| 0.100 - 0.340 % <br>@Time 7200 - 7200 sec |
0.100 - 0.340 % <br>@Time 2.00 - 2.00 hour |
Average value: 0.220 % Grade Count:1 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 4.00 - 95.0 | 4.00 - 95.0 | Average value: 50.9 Grade Count:1151 |
| Hardness, Shore D | 14.5 - 95.2 | 14.5 - 95.2 | Average value: 53.6 Grade Count:12 |
| Hardness, Shore OO | 10.0 - 86.0 | 10.0 - 86.0 | Average value: 52.3 Grade Count:9 |
| Tensile Strength, Ultimate | 0.0552 - 165 MPa | 8.00 - 23900 psi | Average value: 7.09 MPa Grade Count:1176 |
| Tensile Strength, Yield | 0.0448 - 145 MPa | 6.50 - 21000 psi | Average value: 6.06 MPa Grade Count:110 |
| Elongation at Break | 5.00 - 1450 % | 5.00 - 1450 % | Average value: 461 % Grade Count:1167 |
| Elongation at Yield | 0.000 - 240 % | 0.000 - 240 % | Average value: 51.4 % Grade Count:7 |
| Modulus of Elasticity | 0.000517 - 1.90 GPa | 0.0750 - 276 ksi | Average value: 0.0881 GPa Grade Count:27 |
| Compressive Modulus | 0.000200 - 0.00590 GPa | 0.0290 - 0.856 ksi | Average value: 0.00208 GPa Grade Count:10 |
| Poissons Ratio | 0.500 | 0.500 | Average value: 0.500 Grade Count:40 |
| Shear Modulus | 0.0000689 - 1.83 GPa | 0.0100 - 265 ksi | Average value: 0.208 GPa Grade Count:27 |
| Shear Strength | 0.965 - 6.05 MPa | 140 - 878 psi | Average value: 2.92 MPa Grade Count:35 |
| Adhesive Bond Strength | 0.0103 - 0.103 MPa | 1.50 - 15.0 psi | Average value: 0.0462 MPa Grade Count:44 |
| Penetration P(60), 1/10 mm | 36.0 - 135 | 36.0 - 135 | Average value: 70.0 Grade Count:3 |
| Tear Strength | 0.877 - 125 kN/m | 5.00 - 713 pli | Average value: 23.8 kN/m Grade Count:694 |
| 1.5777 - 2.2789 kN/m <br>@Temperature 100 - 150 °C |
9.0024 - 13.003 pli <br>@Temperature 212 - 302 °F |
Average value: 1.93 kN/m Grade Count:1 | |
| Peel Strength | 0.0877 - 7.05 kN/m | 0.500 - 40.2 pli | Average value: 1.30 kN/m Grade Count:376 |
| Compression Set | 3.00 - 77.3 % | 3.00 - 77.3 % | Average value: 23.3 % Grade Count:167 |
| 3.10 - 46.0 % <br>@Temperature 70.0 - 302 °C |
3.10 - 46.0 % <br>@Temperature 158 - 576 °F |
Average value: 22.2 % Grade Count:77 | |
| 3.10 - 46.0 % <br>@Time 79200 - 259000 sec |
3.10 - 46.0 % <br>@Time 22.0 - 72.0 hour |
Average value: 22.2 % Grade Count:77 | |
| Tensile Set | 5.10 - 6.00 % | 5.10 - 6.00 % | Average value: 5.53 % Grade Count:3 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 11.0 - 335 µm/m-°C | 6.11 - 186 µin/in-°F | Average value: 133 µm/m-°C Grade Count:44 |
| 1040 - 1040 µm/m-°C <br>@Temperature 0.000 - 0.000 °C |
578 - 578 µin/in-°F <br>@Temperature 32.0 - 32.0 °F |
Average value: 1040 µm/m-°C Grade Count:1 | |
| CTE, linear, Transverse to Flow | 20.0 - 139 µm/m-°C | 11.1 - 77.2 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:4 |
| Specific Heat Capacity | 0.320 - 1.26 J/g-°C | 0.0765 - 0.301 BTU/lb-°F | Average value: 0.789 J/g-°C Grade Count:20 |
| 0.820 - 0.900 J/g-°C <br>@Temperature 100 - 100 °C |
0.196 - 0.215 BTU/lb-°F <br>@Temperature 212 - 212 °F |
Average value: 0.837 J/g-°C Grade Count:15 | |
| Thermal Conductivity | 0.0600 - 6.50 W/m-K | 0.416 - 45.1 BTU-in/hr-ft²-°F | Average value: 1.09 W/m-K Grade Count:59 |
| 1.00 - 3.3867 W/m-K <br>@Temperature 50.0 - 100 °C |
6.94 - 23.504 BTU-in/hr-ft²-°F <br>@Temperature 122 - 212 °F |
Average value: 2.08 W/m-K Grade Count:15 | |
| 1.50 - 4.69 W/m-K <br>@Temperature 50.0 - 50.0 °C |
10.4 - 32.5 BTU-in/hr-ft²-°F <br>@Temperature 122 - 122 °F |
Average value: 2.08 W/m-K Grade Count:4 | |
| 1.50 - 4.69 W/m-K <br>@Pressure 30.0 - 30.0 MPa |
10.4 - 32.5 BTU-in/hr-ft²-°F <br>@Pressure 4350 - 4350 psi |
Average value: 2.08 W/m-K Grade Count:4 | |
| Maximum Service Temperature, Air | 93.3 - 315 °C | 200 - 599 °F | Average value: 223 °C Grade Count:644 |
| Maximum Service Temperature, Inert | 154 - 260 °C | 310 - 500 °F | Average value: 221 °C Grade Count:59 |
| Minimum Service Temperature, Air | -136 - -40.0 °C | -212 - -40.0 °F | Average value: -58.4 °C Grade Count:672 |
| Brittleness Temperature | -73.0 - -65.0 °C | -99.4 - -85.0 °F | Average value: -70.3 °C Grade Count:3 |
| Glass Transition Temp, Tg | -120 - 118 °C | -184 - 244 °F | Average value: -106 °C Grade Count:37 |
| UL RTI, Electrical | 65.6 - 220 °C | 150 - 428 °F | Average value: 210 °C Grade Count:135 |
| UL RTI, Mechanical without Impact | 65.6 - 220 °C | 150 - 428 °F | Average value: 202 °C Grade Count:135 |
| Flammability, UL94 | HB - V-0 | HB - V-0 | Grade Count:217 |
| HB - HB <br>@Temperature 200 - 220 °C |
HB - HB <br>@Temperature 392 - 428 °F |
Grade Count:15 | |
| Flash Point | -4.00 - 100 °C | 24.8 - 212 °F | Average value: 33.0 °C Grade Count:4 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00500 - 9.00e+15 ohm-cm | 0.00500 - 9.00e+15 ohm-cm | Average value: 1.04e+15 ohm-cm Grade Count:63 |
| Shielding Effectiveness | 55.0 - 141 dB | 55.0 - 141 dB | Average value: 100 dB Grade Count:5 |
| Dielectric Constant | 2.20 - 35.0 | 2.20 - 35.0 | Average value: 13.9 Grade Count:70 |
| 2.50 - 3.00 <br>@Temperature 90.0 - 150 °C |
2.50 - 3.00 <br>@Temperature 194 - 302 °F |
Average value: 20.8 Grade Count:9 | |
| 24.5 - 27.7 <br>@Temperature 65.0 - 90.0 °C |
24.5 - 27.7 <br>@Temperature 149 - 194 °F |
Average value: 20.8 Grade Count:8 | |
| 24.5 - 27.7 <br>@Frequency 60.0 - 60.0 Hz |
24.5 - 27.7 <br>@Frequency 60.0 - 60.0 Hz |
Average value: 20.8 Grade Count:8 | |
| Dielectric Strength | 1.14 - 118 kV/mm | 29.0 - 3000 kV/in | Average value: 21.5 kV/mm Grade Count:567 |
| Dissipation Factor | 0.0000230 - 0.900 | 0.0000230 - 0.900 | Average value: 0.126 Grade Count:65 |
| 0.500 - 0.700 <br>@Temperature 130 - 150 °C |
0.500 - 0.700 <br>@Temperature 266 - 302 °F |
Average value: 0.600 Grade Count:1 | |
| Arc Resistance | 60.0 - 193 sec | 60.0 - 193 sec | Average value: 163 sec Grade Count:5 |
| Track Resistance | 3600 - 36000 sec | 3600 - 36000 sec | Average value: 22300 sec Grade Count:17 |