Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000500 - 0.00500 cm/cm | 0.000500 - 0.00500 in/in | Average value: 0.00215 cm/cm Grade Count:15 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00500 cm/cm | 0.000 - 0.00500 in/in | Average value: 0.00133 cm/cm Grade Count:40 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00269 cm/cm Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00309 cm/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00288 cm/cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IPM2000 PMMA- ABS Alloy High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00232 cm/cm Grade Count:21 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00500 - 0.00500 cm/cm @Temperature 80.0 - 80.0 °C |
0.00500 - 0.00500 in/in @Temperature 176 - 176 °F |
Average value: 0.00500 cm/cm Grade Count:1 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |