Bhansali Engineering Santron IMS1000M SAN Resin

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer Bhansali Engineering
Trade Name Santron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bhansali Engineering Santron IMS1000M SAN Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Clear SAN, Pen barrel applicationInformation provided by Bhansali
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Melt Flow 35.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 63.7 MPa

@Thickness 3.20 mm
9250 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
68.6 MPa

@Thickness 3.20 mm
9960 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 98.1 MPa

@Thickness 6.40 mm
14200 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Izod Impact, Notched 0.294 J/cm

@Thickness 3.20 mm
0.551 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
Method A; ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Optical Properties Metric English Comments
Transmission, Visible 90.0 %
90.0 %
clear; thickness not quantified