Physical Properties Metric English Comments
Apparent Bulk Density 0.360 - 0.420 g/cc
0.0130 - 0.0152 lb/in³
NanoAmor 95%, OD/ID/L: 8-15/3-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Apparent Bulk Density 0.360 - 0.950 g/cc
0.0130 - 0.0343 lb/in³
Average value: 0.665 g/cc Grade Count:26
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Apparent Bulk Density 0.360 g/cc
0.0130 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..