Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 180 g/10 min | 180 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Melt Flow | 180 g/10 min @Load 5.00 kg, Temperature 260 °C |
180 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Mitsui TPX® DX820 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |