| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow |
21
g/10 min <br>@Load 21.6 kg,<br> Temperature 190 °C
|
21
g/10 min <br>@Load 47.6 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding
Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 190 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Polimeri Europa Eraclene® MP 94 U High Density Polyethylene - Injection Molding
Eraclene MP 94 U is a gas phase high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
21
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ISO 1133 |
|
SABIC Innovative Plastics Cycolac® INP630 ABS
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
21
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
ISO 1133 |
|
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 260 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 500 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 220 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 428 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Lexan® VR2020 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C
|
21
g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F
|
Index; ASTM-D1238 |
|
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200R PC
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200R PC (Asia Pacific)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2203R PC
PC2203R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 220 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 428 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Ultem 1110FV PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 360 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 680 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Ultem 1110R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 360 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 680 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 360 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 680 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D 1238 |
|
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 10.0 kg,<br> Temperature 200 °C
|
21
g/10 min <br>@Load 22.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Techmer ES Plastiblend® ABS NAT
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 5.00 kg,<br> Temperature 360 °C
|
21
g/10 min <br>@Load 11.0 lb,<br> Temperature 680 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 265 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 509 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East)
XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C
|
|||
| Melt Flow |
21
g/10 min <br>@Load 10.0 kg,<br> Temperature 200 °C
|
21
g/10 min <br>@Load 22.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Techmer ES Plastiblend® ABS LE BK
Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
cm³/10min; ISO 1133 |
|
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**)
Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
21
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
cm³/10min; ISO 1133 |
|
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
|
|||
| Melt Flow |
21
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
21
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
|
SABIC Innovative Plastics PC2200 PC
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||