Mechanical Properties Metric English Comments
Modulus of Elasticity 1.90 - 2.20 GPa

@Temperature 60.0 - 90.0 °C
276 - 319 ksi

@Temperature 140 - 194 °F
Average value: 2.05 GPa Grade Count:1
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 1.70 - 2.20 GPa

@Temperature 60.0 - 120 °C
247 - 319 ksi

@Temperature 140 - 248 °F
Average value: 1.93 GPa Grade Count:1
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.640 - 2.20 GPa

@Temperature 60.0 - 150 °C
92.8 - 319 ksi

@Temperature 140 - 302 °F
Average value: 1.21 GPa Grade Count:1
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Modulus of Elasticity 0.200 - 2.20 GPa
29.0 - 319 ksi
Average value: 1.02 GPa Grade Count:20
Overview of materials for Nylon, Flexible Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 1.60 - 2.20 GPa
232 - 319 ksi
Average value: 1.90 GPa Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Modulus of Elasticity 0.483 - 2.20 GPa
70.1 - 319 ksi
Average value: 1.31 GPa Grade Count:3
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..