| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Overview of materials for Nylon 66, Glass Bead Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.890 - 1.75 g/cc | 0.0322 - 0.0632 lb/in³ | Average value: 1.37 g/cc Grade Count:108 |
| Filler Content | 5.00 - 40.0 % | 5.00 - 40.0 % | Average value: 21.4 % Grade Count:20 |
| Water Absorption | 0.0500 - 5.60 % | 0.0500 - 5.60 % | Average value: 0.941 % Grade Count:44 |
| Moisture Absorption at Equilibrium | 0.250 - 4.40 % | 0.250 - 4.40 % | Average value: 2.13 % Grade Count:14 |
| Water Absorption at Saturation | 4.50 - 9.45 % | 4.50 - 9.45 % | Average value: 6.14 % Grade Count:4 |
| Linear Mold Shrinkage | 0.00150 - 0.0280 cm/cm | 0.00150 - 0.0280 in/in | Average value: 0.0124 cm/cm Grade Count:100 |
| Linear Mold Shrinkage, Transverse | 0.00630 - 0.0170 cm/cm | 0.00630 - 0.0170 in/in | Average value: 0.0114 cm/cm Grade Count:21 |
| Melt Flow | 1.00 - 3.00 g/10 min | 1.00 - 3.00 g/10 min | Average value: 2.00 g/10 min Grade Count:8 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 98.0 - 122 | 98.0 - 122 | Average value: 118 Grade Count:29 |
| Tensile Strength, Ultimate | 38.0 - 150 MPa | 5510 - 21800 psi | Average value: 78.2 MPa Grade Count:87 |
| 25.0 - 55.0 MPa @Temperature 60.0 - 150 °C |
3630 - 7980 psi @Temperature 140 - 302 °F |
Average value: 38.4 MPa Grade Count:2 | |
| Tensile Strength, Yield | 50.0 - 131 MPa | 7250 - 19000 psi | Average value: 87.4 MPa Grade Count:27 |
| Elongation at Break | 0.500 - 20.0 % | 0.500 - 20.0 % | Average value: 4.68 % Grade Count:99 |
| 15.0 - 45.0 % @Temperature 60.0 - 150 °C |
15.0 - 45.0 % @Temperature 140 - 302 °F |
Average value: 26.3 % Grade Count:1 | |
| Elongation at Yield | 2.40 - 11.0 % | 2.40 - 11.0 % | Average value: 5.03 % Grade Count:10 |
| 10.0 - 16.0 % @Temperature 60.0 - 150 °C |
10.0 - 16.0 % @Temperature 140 - 302 °F |
Average value: 13.8 % Grade Count:1 | |
| Modulus of Elasticity | 1.70 - 10.0 GPa | 247 - 1450 ksi | Average value: 4.74 GPa Grade Count:75 |
| 0.640 - 2.20 GPa @Temperature 60.0 - 150 °C |
92.8 - 319 ksi @Temperature 140 - 302 °F |
Average value: 1.21 GPa Grade Count:1 | |
| Flexural Yield Strength | 58.6 - 207 MPa | 8500 - 30000 psi | Average value: 130 MPa Grade Count:89 |
| Flexural Modulus | 2.48 - 10.3 GPa | 360 - 1500 ksi | Average value: 4.62 GPa Grade Count:97 |
| 1.25 - 3.05 GPa @Temperature 60.0 - 120 °C |
181 - 442 ksi @Temperature 140 - 248 °F |
Average value: 1.97 GPa Grade Count:1 | |
| Compressive Yield Strength | 31.0 - 68.9 MPa | 4500 - 10000 psi | Average value: 49.6 MPa Grade Count:8 |
| Izod Impact, Notched | 0.214 - 0.694 J/cm | 0.400 - 1.30 ft-lb/in | Average value: 0.409 J/cm Grade Count:59 |
| 0.350 - 0.350 J/cm @Temperature -40.0 - -20.0 °C |
0.656 - 0.656 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.350 J/cm Grade Count:1 | |
| Izod Impact, Unnotched | 1.01 - 6.41 J/cm | 1.90 - 12.0 ft-lb/in | Average value: 3.16 J/cm Grade Count:40 |
| Izod Impact, Notched (ISO) | 1.50 - 8.00 kJ/m² | 0.714 - 3.81 ft-lb/in² | Average value: 4.30 kJ/m² Grade Count:30 |
| 2.00 - 7.00 kJ/m² @Temperature -40.0 - -20.0 °C |
0.952 - 3.33 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.71 kJ/m² Grade Count:5 | |
| Izod Impact, Unnotched (ISO) | 20.0 - 55.0 kJ/m² | 9.52 - 26.2 ft-lb/in² | Average value: 28.3 kJ/m² Grade Count:11 |
| 18.0 - 50.0 kJ/m² @Temperature -30.0 - -30.0 °C |
8.57 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 31.0 kJ/m² Grade Count:3 | |
| Charpy Impact Unnotched | 1.00 - 6.00 J/cm² | 4.76 - 28.6 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:31 |
| 1.00 - 4.50 J/cm² @Temperature -40.0 - -20.0 °C |
4.76 - 21.4 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.58 J/cm² Grade Count:12 | |
| Charpy Impact, Notched | 0.200 - 1.80 J/cm² | 0.952 - 8.57 ft-lb/in² | Average value: 0.617 J/cm² Grade Count:27 |
| 0.0800 - 0.800 J/cm² @Temperature -30.0 - -20.0 °C |
0.381 - 3.81 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.478 J/cm² Grade Count:10 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.00 - 73.8 µm/m-°C | 3.33 - 41.0 µin/in-°F | Average value: 50.9 µm/m-°C Grade Count:41 |
| CTE, linear, Transverse to Flow | 30.0 - 86.0 µm/m-°C | 16.7 - 47.8 µin/in-°F | Average value: 54.6 µm/m-°C Grade Count:8 |
| Thermal Conductivity | 0.250 - 0.389 W/m-K | 1.74 - 2.70 BTU-in/hr-ft²-°F | Average value: 0.316 W/m-K Grade Count:12 |
| Melting Point | 254 - 265 °C | 489 - 509 °F | Average value: 258 °C Grade Count:43 |
| Maximum Service Temperature, Air | 80.0 - 180 °C | 176 - 356 °F | Average value: 126 °C Grade Count:4 |
| Deflection Temperature at 0.46 MPa (66 psi) | 190 - 260 °C | 374 - 500 °F | Average value: 230 °C Grade Count:56 |
| Deflection Temperature at 1.8 MPa (264 psi) | 61.0 - 250 °C | 142 - 482 °F | Average value: 156 °C Grade Count:95 |
| Vicat Softening Point | 225 - 255 °C | 437 - 491 °F | Average value: 241 °C Grade Count:25 |
| Flammability, UL94 | HB - V-0 | HB - V-0 | Grade Count:72 |
| Oxygen Index | 26.0 - 33.0 % | 26.0 - 33.0 % | Average value: 27.7 % Grade Count:6 |
| Glow Wire Test | 650 °C | 1200 °F | Average value: 650 °C Grade Count:12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+12 - 1.00e+17 ohm-cm | 1.00e+12 - 1.00e+17 ohm-cm | Average value: 3.65e+15 ohm-cm Grade Count:61 |
| Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.59e+14 ohm Grade Count:24 |
| Dielectric Constant | 3.60 - 6.00 | 3.60 - 6.00 | Average value: 4.23 Grade Count:22 |
| Dielectric Strength | 15.0 - 80.0 kV/mm | 380 - 2030 kV/in | Average value: 28.9 kV/mm Grade Count:46 |
| Dissipation Factor | 0.0100 - 0.0200 | 0.0100 - 0.0200 | Average value: 0.0159 Grade Count:11 |
| Dielectric Loss Index | 0.0150 - 0.150 | 0.0150 - 0.150 | Average value: 0.0825 Grade Count:8 |
| Comparative Tracking Index | 250 - 600 V | 250 - 600 V | Average value: 470 V Grade Count:24 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 284 °C Grade Count:25 |
| Nozzle Temperature | 250 - 304 °C | 482 - 580 °F | Average value: 277 °C Grade Count:9 |
| Melt Temperature | 241 - 310 °C | 465 - 590 °F | Average value: 281 °C Grade Count:55 |