Polymer Property : Modulus of Elasticity = 377 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.50 - 2.60 GPa

@Temperature -18.0 - 71.0 °C
218 - 377 ksi

@Temperature -0.400 - 160 °F
Average value: 2.05 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Modulus of Elasticity 2.00 - 2.60 GPa
290 - 377 ksi
Average value: 2.35 GPa Grade Count:63
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 1.72 - 2.60 GPa
250 - 377 ksi
Average value: 2.18 GPa Grade Count:25
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Modulus of Elasticity 1.70 - 2.60 GPa
247 - 377 ksi
Average value: 2.26 GPa Grade Count:5
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..