Polymer Property : Modulus of Elasticity = 1800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 12.4 GPa
1800 ksi
ASTM D638
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Modulus of Elasticity 12.4 GPa
1800 ksi
ASTM D638
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade
Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II.
Modulus of Elasticity 12.4 - 28.0 GPa
1800 - 4060 ksi
Average value: 21.5 GPa Grade Count:4
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Modulus of Elasticity 12.4 - 45.0 GPa
1800 - 6530 ksi
Average value: 33.5 GPa Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Modulus of Elasticity 12.4 GPa
1800 ksi
ASTM D638
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Modulus of Elasticity 12.4 GPa
1800 ksi
Sawbones E-Glass-Filled Epoxy Sheets
Primary UseE-glass-filled epoxy sheets are primarily used as an alternative test medium to human cortical bone.DescriptionE-glass-filled epoxy sheets are a mixture of short e-glass fibers and epoxy ..
Modulus of Elasticity 12.4 GPa
1800 ksi
Sawbones Third-Generation Simulated Cortical Bone
E-glass-filled EpoxySawbones® Third-Generation Bones model natural cortical bone using a mixture of short e-glass fibers and epoxy resin pressure injected around a foam core. The mid-shaft area h..
Modulus of Elasticity 12.4 GPa
1800 ksi
ASTM D638
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Modulus of Elasticity 12.4 GPa
1800 ksi
Sawbones E-Glass-Filled Epoxy Cylinders
Primary UseE-glass-filled epoxy cylinders are primarily used as an alternative test medium to human cortical bone.DescriptionThey are a mixture of short e-glass fibers and epoxy resin that has been ..
Modulus of Elasticity 12.4 GPa
1800 ksi
ASTM C580
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..
Modulus of Elasticity 12.4 GPa
1800 ksi
Flexural
Chesterton ARC NVE SYSTEM Vinyl Ester Lining
Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i..