Polymer Property : Flexural Strength = 172 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 159 - 172 MPa
23000 - 25000 psi
ASTM D790
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Strength 34.5 - 172 MPa
5000 - 25000 psi
Du-Co Ceramics S-699 Alumina
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Flexural Strength 159 - 172 MPa
23000 - 25000 psi
Bulk Molding Compounds BMC 1412 Flame and Track Resistant
BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu..
Flexural Strength 138 - 172 MPa
20000 - 25000 psi
Bulk Molding Compounds BMC 8005 Polyester Molding Compound
Flexural Strength 138 - 172 MPa
20000 - 25000 psi
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..