Polymer Property : Flexural Strength = 70.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 70.0 MPa
10200 psi
Plastcom SLOVAMID 66 HI/1 TS PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Flexural Strength 70.0 MPa
10200 psi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nima™ NH PC143P Polycarbonate
Non-Hal FR-PC with High impact and improved processabilityAll properties after 48hrs conditioning at 23°C/50% RH
Flexural Strength 70.0 - 90.0 MPa
10200 - 13100 psi
Compression; ISO 178
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Flexural Strength 70.0 - 100 MPa
10200 - 14500 psi
Compression; ISO 178
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Flexural Strength 70.0 MPa
10200 psi
Reliance Industries Polypropylene - 30% glass fiber filled
Information provided by Reliance Industries
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Nilit FRIANYL B63 D-S10 Nylon 6., std. viscosity for injection molding
Nylon 6., std. viscosity for injection molding, permanently flexible, increased dry impact resistance (for dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Strength 70.0 MPa
10200 psi
ISO 178
BASF Capron® 8224 HSL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Strength 70.0 MPa
10200 psi
Lehmann & Voss LUVOCOM® 80-8318-1 Polyacetal-copolymer, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Flexural Strength 70.0 MPa
10200 psi
2mm/min; ASTM D790
Kingfa PBT-T15 15% Mineral Filled PBT
Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Flexural Strength 70.0 MPa
10200 psi
2 mm/min; ISO 178
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet
PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
Flexural Strength 70.0 MPa
<br>@Temperature 23.0 °C
10200 psi
<br>@Temperature 73.4 °F
2mm/min; 80x10x4mm; ISO 178
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS)
High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Solvay TECHNYL® C 50 H2 PA6, Conditioned
Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This p..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Styrolution Novodur® 4115 ABS
Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Styrolution Polystyrol 145 D PS
Description: Polystyrol 145 D is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol.Applications: In blends with high impact polystyrene esp..
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D..
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Polyram RamLloy B001 Nylon 6/Polyolefin Alloy, Impact Modified
Nylon 6/Polyolefin alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram.
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman.
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene
DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Eurostar Star L POM D36 POM, Injection Molded
Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Eurostar Star L POM D74 POM, Injection Molded
Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Flexural Strength 70.0 MPa
10200 psi
SAE J949
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Ashley Polymers Ashlene® F242 ABS
Flame retardant.Data provided by the manufacturer
Flexural Strength 70.0 - 110 MPa
10200 - 16000 psi
ISO 178
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound
Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm..
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Ashley Polymers Ashlene® 256 PPO
A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer
Flexural Strength 70.0 MPa
10200 psi
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
Flexural Strength 70.0 MPa
10200 psi
ISO 178-93
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
Flexural Strength 70.0 MPa
10200 psi
23°C, 50% RH; ASTM D790
Asahi Kasei Xyron® 300V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Polyram RamShine PAS703 ASA, UV Stabilized
Is a general purpose injection molding ASA, good chemical resistance, UV stabilization.Information provided by Polyram.
Copyright © lookpolymers.com All Rights Reserved