Mechanical Properties Metric English Comments
Puncture Energy 41.0 J

@Temperature -40.0 °C
30.2 ft-lb

@Temperature -40.0 °F
ISO 6603-2
Borealis BC650MO Polypropylene Copolymer
BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig..
Puncture Energy 41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles
Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis..
Puncture Energy 41.0 J

@Temperature 0.000 °C
30.2 ft-lb

@Temperature 32.0 °F
At Max load; ASTM D3763
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles
Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis..
Puncture Energy 41.0 J

@Thickness 2.50 mm,
Temperature -40.0 °C
30.2 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Puncture Energy 41.0 J

@Thickness 2.50 mm,
Temperature -40.0 °C
30.2 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
At Max load; ASTM D3763
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Puncture Energy 41.0 J

@Temperature 23.0 °C
30.2 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
Eastman Spectar® Clear Copolyester for Thermoforming