Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 46.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 46.0 J

@Temperature -20.0 °C
33.9 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BC650MO Polypropylene Copolymer
BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig..
Puncture Energy 46.0 J

@Temperature -40.0 °C
33.9 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
Eastman Eastar DN001HF Copolyester
Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p..
Puncture Energy 46.0 J

@Temperature -40.0 °C
33.9 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
Eastman Eastar DN004HF Copolyester
Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p..
Puncture Energy 46.0 J

@Temperature 23.0 °C
33.9 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Bayblend® T85 SG PC/ABS Blend