| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | DIN 53453 |
|
Nilit FRIANYL A63 HH-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature 23.0 °C
|
2.14
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Victrex® PEEK 90G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
|
|||
| Charpy Impact, Notched | 0.450 - 0.750 J/cm² | 2.14 - 3.57 ft-lb/in² | Average value: 0.650 J/cm² Grade Count:3 |
|
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | Dried; ISO 179 |
|
Manifattura Cattaneo PA 6.6 Nylon
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -30.0 °C
|
2.14
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1EA |
|
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM
Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -20.0 °C
|
2.14
ft-lb/in² <br>@Temperature -4.00 °F
|
DIN 53453 |
|
IRPC Polimaxx Polene 2346S Polypropylene Block Copolymer
CHARACTERISTICS: HIGH STIFFNESS, HIGH FLOW, GOOD IMPACT, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature 23.0 °C
|
2.14
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Grupo Repol Dinalon® B1S25 G10B20 PA6 10% Glass Fiber, 20% Glass Beads
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | |
|
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa..
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | |
|
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced
EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature 23.0 °C
|
2.14
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/1eA |
|
Borealis HA104E Polypropylene Homopolymer
HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -20.0 °C
|
2.14
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179/1eA |
|
Borealis Xmod™ BE677AI High Crystalline Polypropylene Copolymer
Xmod BE677AI is a UV-stabilized HCPP intended for injection molding of automotive interior and appliance parts. Xmod BE677AI has an excellent balance between impact strength and stiffness as well ..
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ASTM D256 |
|
Plenco 6582 Phenolic, Briquette, Transfer Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -20.0 °C
|
2.14
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 179 |
|
Total PPC 12712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature 30.0 °C
|
2.14
ft-lb/in² <br>@Temperature 86.0 °F
|
conditioned; ISO 179/1eU |
|
EMS-Grivory Grivory® TSM-30/2 PA666-MD30
Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -40.0 °C
|
2.14
ft-lb/in² <br>@Temperature -40.0 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont ..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature 23.0 °C
|
2.14
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® RS LC3030 NC010 Nylon 610
(Unverified Data**)
Zytel® RS LC3030 NC010 is a renewable sourced polyamide 610 containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, low viscosity grade, developed for extrusion a..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -40.0 °C
|
2.14
ft-lb/in² <br>@Temperature -40.0 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | |
|
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -30.0 °C
|
2.14
ft-lb/in² <br>@Temperature -22.0 °F
|
|
|
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Dry)
Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High ..
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179-1eA |
|
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection
PBT-MD30Information provided by BARLOG plastics GmbH.
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179 1eA |
|
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
|
|||
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | dry; ISO 179 1eA |
|
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored
Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac..
|
|||
| Charpy Impact, Notched |
0.450
-
1.90
J/cm² <br>@Temperature -30.0 - -30.0 °C
|
2.14
-
9.04
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 1.16 J/cm² Grade Count:54 |
|
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
|
|||
| Charpy Impact, Notched |
0.450
J/cm² <br>@Temperature -30.0 °C
|
2.14
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1EA |
|
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH
Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri..
|
|||