Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.476 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.100 J/cm²

@Temperature 23.0 °C
0.476 ft-lb/in²

@Temperature 73.4 °F
ISO 179/2C
SABIC Innovative Plastics Cycolac® INP563 ABS
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN
SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN
INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi..
Charpy Impact, Notched 0.100 - 0.200 J/cm²
0.476 - 0.952 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Charpy Impact, Notched 0.100 J/cm² - NB
0.476 ft-lb/in² - NB
Average value: 1.18 J/cm² Grade Count:147
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Cycolac® INP581 ABS+SAN
High flow, low molecular weight SAN. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for..
Charpy Impact, Notched 0.100 - 4.80 J/cm²

@Temperature -40.0 - 0.000 °C
0.476 - 22.8 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 0.394 J/cm² Grade Count:108
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Charpy Impact, Notched 0.100 - 1.00 J/cm²

@Temperature -30.0 - 30.0 °C
0.476 - 4.76 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.430 J/cm² Grade Count:22
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Charpy Impact, Notched 0.100 - 1000 J/cm²
0.476 - 4760 ft-lb/in²
Average value: 1.21 J/cm² Grade Count:161
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.100 - 3.10 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 14.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.690 J/cm² Grade Count:100
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced
Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled
Dissipative product based on Polypropylene homopolymer (PPh). Mica filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Charpy Impact, Notched 0.100 J/cm²

@Temperature 23.0 °C
0.476 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
Charpy Impact, Notched 0.100 J/cm²

@Temperature 23.0 °C
0.476 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
Charpy Impact, Notched 0.100 - 0.200 J/cm²
0.476 - 0.952 ft-lb/in²
ISO 179
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO Data, Low Temp
Dow Tyril® 125 SAN
Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO Data, Low Temp
Dow Tyril® 1000B SAN
TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good ..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
DIN 53453
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Charpy Impact, Notched 0.100 J/cm²

@Temperature 23.0 °C
0.476 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP
SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications...
Charpy Impact, Notched 0.100 - 0.800 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.425 J/cm² Grade Count:4
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Charpy Impact, Notched 0.100 - 0.600 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 2.86 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.193 J/cm² Grade Count:46
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Charpy Impact, Notched 0.100 J/cm²
0.476 ft-lb/in²
ISO Data, Low Temp
Americas Styrenics Styron® 612 Polystyrene  (discontinued **)
STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, ..
Charpy Impact, Notched 0.100 - 12.0 J/cm²

@Temperature -30.0 - 0.000 °C
0.476 - 57.1 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 1.91 J/cm² Grade Count:27
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.100 - 2.00 J/cm²

@Temperature -40.0 - -20.0 °C
0.476 - 9.52 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.596 J/cm² Grade Count:39
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Copyright © lookpolymers.com All Rights Reserved