| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179/2C |
|
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -30.0 °C
|
8.57
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179/1eA |
|
Nilit FRIANYL B63 L-HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
Polykemi AB SCANMID 6 B22^ E F40 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -30.0 °C
|
8.57
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 179 |
|
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
|
Ineos ABS Lustran® H606 LS
Improved heat and UV resistance.,Property data per ISO test methods.
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eU |
|
Lucite International Diakon® CLG340 Acrylic Polymer
Information provided by Lucite International
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | |
|
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -30.0 °C
|
8.57
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4mm, Cut; ISO 179/1eA |
|
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP
SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
|
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 30.0 °C
|
8.57
ft-lb/in² <br>@Temperature 86.0 °F
|
dry; ISO 179/1eU |
|
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50
Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E..
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
CP-Polymer-Technik Wellamid® 6000 SUVCP Nylon 6, Finely Crystalline, UV Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60
Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | conditioned; ISO 179/1eA |
|
EMS-Grivory Grivory® XE 3959 black 9992 PA610
Product description: Grilamid XE 3959 is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and i..
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -40.0 °C
|
8.57
ft-lb/in² <br>@Temperature -40.0 °F
|
DAM; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -30.0 °C
|
8.57
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
|
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)
(Unverified Data**)
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
|
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
|
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO179 |
|
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin
15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | Conditioned; ISO 179/IeA |
|
Addiplast Addinyl C2 V40 Nylon 66/6, 40% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature 23.0 °C
|
8.57
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 179 |
|
BASF Ultramid® A3W2G6 BK 20560 30% Glass Filled PA66 (Conditioned)
Description: Ultramid A3W2G6 BK20560 is a developmental 30% glass fiber reinforced, pigmented black, injection molding PA66/6 with high heat aging resistance.Applications: Automotive power train app..
|
|||
| Charpy Impact, Notched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eA |
|
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned)
Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade.
|
|||
| Charpy Impact, Notched |
1.80
J/cm² <br>@Temperature -30.0 °C
|
8.57
ft-lb/in² <br>@Temperature -22.0 °F
|
50%RH; ISO 179/1eA |
|
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**)
40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex..
|
|||