Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.00 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
1.87 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Polimeri Europa Edistir R 540E Polystyrene
HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection moldings. Designation: Thermoplastics IS..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
Izod Impact, Notched 1.00 J/cm

@Temperature -30.0 °C
1.87 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched 1.00 J/cm

@Temperature -30.0 °C
1.87 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Asia Pacific)
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched 1.00 - 1.00 J/cm

@Temperature 0.000 - 0.000 °C
1.87 - 1.87 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.960 J/cm Grade Count:2
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256A
LyondellBasell Pro-fax SB787 Polypropylene Impact Copolymer
Key Features: blush resistance, excellent dimensional satiability, fast cycling, easy molding, good cold impact resistance, good stiffness and impact balance, easily colored, FDA acceptableApplicati..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256-03
Ipiranga Petrochem PCC 0742 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Kuraray Genestarâ„¢ GT2330 Nylon, 33% Glass Filled
Toughness V-0 Grade. It is well suited for components requiring a high strength in pin fitting process, due to high ductility properties.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Asia Pacific)
RN0401 is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 20% PCR styrenic series resin content. Available in black only.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Shuman 880 Grey Polystyrene High Impact
Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
Izod Impact, Notched 1.00 J/cm

@Thickness 3.20 mm
1.87 ft-lb/in

@Thickness 0.126 in
ASTM D256
Supreme Petrochem SP 554 Flame Retardant Polystyrene
Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman.
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PA810 Nylon 6.6, Impact Modified
Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PA840G3 Nylon 6.6, 15% Glass Fiber
15% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman.
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamSter PF320G6 PBT, 30% Glass Fiber, Flame Retardant
30% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Toyobo Vylopet® EMC615 PET/PBT Blend
Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go..
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM
GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
Izod Impact, Notched 1.00 J/cm

@Diameter 3.17 mm
1.87 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
BP Amoco Acclear® 8439 Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Low bloomingTypical applications: Housewares, Rigid packagingComplies with FDA specif..