Polymer Property : Izod Impact, Unnotched = 25.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.497 - 13.3 J/cm
0.930 - 25.0 ft-lb/in
Average value: 6.94 J/cm Grade Count:7
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Unnotched 1.44 - 13.3 J/cm
2.70 - 25.0 ft-lb/in
Average value: 4.11 J/cm Grade Count:27
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Izod Impact, Unnotched 2.51 - 13.3 J/cm
4.70 - 25.0 ft-lb/in
Average value: 4.72 J/cm Grade Count:12
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Izod Impact, Unnotched 3.74 - 13.3 J/cm
7.00 - 25.0 ft-lb/in
Average value: 6.86 J/cm Grade Count:10
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Izod Impact, Unnotched 1.17 - 13.3 J/cm
2.20 - 25.0 ft-lb/in
Average value: 5.86 J/cm Grade Count:31
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Izod Impact, Unnotched 3.74 - 13.3 J/cm
7.00 - 25.0 ft-lb/in
Average value: 7.85 J/cm Grade Count:74
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 1.33 - 13.3 J/cm
2.50 - 25.0 ft-lb/in
Average value: 7.27 J/cm Grade Count:97
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 9.08 - 13.3 J/cm
17.0 - 25.0 ft-lb/in
Average value: 10.7 J/cm Grade Count:5
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Unnotched 2.67 - 13.3 J/cm
5.00 - 25.0 ft-lb/in
Average value: 7.52 J/cm Grade Count:25
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Unnotched 3.74 - 13.3 J/cm
7.00 - 25.0 ft-lb/in
Average value: 7.98 J/cm Grade Count:54
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Izod Impact, Unnotched 2.40 - 13.3 J/cm
4.50 - 25.0 ft-lb/in
Average value: 5.97 J/cm Grade Count:14
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..