Izod Impact, Notched (ISO) 5.70 - 7.21 kJ/m²
2.71 - 3.43 ft-lb/in²
Average value: 6.60 kJ/m² Grade Count:10
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched (ISO) 5.70 - 8.00 kJ/m²
2.71 - 3.81 ft-lb/in²
Average value: 6.67 kJ/m² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Izod Impact, Notched (ISO) 5.70 kJ/m²

@Temperature 23.0 °C
2.71 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Aardvark Polymers AARTEL® 800 Rotational Molding Resin
Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st..
Izod Impact, Notched (ISO) 5.70 kJ/m²
2.71 ft-lb/in²
Sample Type A; ISO 180:2000
Global EPP PA 66E Extruded Polyamide 66
Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu..
Izod Impact, Notched (ISO) 5.70 kJ/m²
2.71 ft-lb/in²
ISO 180-A
Ecomass® 1950ZC84 Stainless Steel Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyamide (PA6/10)Very Good ToughnessInformation provided by Technical Polym..
Izod Impact, Notched (ISO) 5.70 - 28.5 kJ/m²
2.71 - 13.6 ft-lb/in²
Average value: 15.5 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched (ISO) 5.70 kJ/m²
2.71 ft-lb/in²
GBT1043
Beijing Evergrow Resources MC Nylon
Information provided by Beijing Evergrow Resources.
Izod Impact, Notched (ISO) 5.70 kJ/m²
2.71 ft-lb/in²
ISO 180
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant  (discontinued **)&l
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..