| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature -30.0 °C |
2.86
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East)
GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature -30.0 °C |
2.86
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HFD4211 PC
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU (Europe-Africa-Middle East)
LNP* COLORCOMP* G1000-GY4A805-0 is a compound based on Polysulfone resin. Added features include: Custom Color Grey.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK
LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP OCL36AXP PPS (Europe-Africa-Middle East)
LNP* LUBRICOMP* OCL36AXP is a compound based on PPS-Branched resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific)
LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON WE003ER PBT (Europe-Africa-Middle East)
LNP* Stat-kon* WE003ER is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Easy Release, Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature 23.0 °C |
2.86
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI
LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature 23.0 °C |
2.86
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific)
LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP OF008AH PPS - Branched
LNP* THERMOCOMP* OF008AH is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added features of this grade are: Healthcare.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66
LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature -30.0 °C |
2.86
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature -30.0 °C |
2.86
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² @Temperature -30.0 °C |
2.86
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics ULTEM 9090 PEI
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® SHF4930 PBT
Super high flow FR PBT grade with 15% Glass reinforced
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180 |
|
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 234 is an injection molding grade, 20% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance, high stiffness and lo..
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180 |
|
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film
Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P..
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180-A |
|
Ecomass® 4301ZC82 Stainless Steel Filled Polyphthalamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsStainless Steel Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Po..
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180 |
|
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180/1A |
|
Addiplast Addilene H 210 Polypropylene Homopolymer
UnreinforcedInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | ISO 180 |
|
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
|
|||