Polymer Property : Tensile Strength, Yield = 22.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.5 MPa
3260 psi
ASTM D638
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin
Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid..
Tensile Strength, Yield 22.5 MPa
3260 psi
Kraton® D1102 + PP blend (25/75)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Tensile Strength, Yield 22.5 MPa
3260 psi
50mm/min; ISO 527-2
Borealis BC650MO Polypropylene Copolymer
BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig..
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Tensile Strength, Yield >= 22.5 MPa
>= 3270 psi
2 in/min; ASTM D638
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved