Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
Rotuba MSS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
3M Dyneon™ THV 220A Fluorothermoplastic
(discontinued **) THV 220A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate. It is soluble in ketones, esters, or ether.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
3M Dyneon™ THV 220G Fluorothermoplastic
(discontinued **) THV 220G is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. IT proves a balance of low temperature process.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178 |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA 10 A is a thermoplastic polyolefin which has been developed for the extrusion and calendering of soft film and sheet. Thanks to its high rubber content "Hifax" CA 10 A fe.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD801A PPE-TPE (Europe-Africa-Middle East) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MH 2030 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MH 2030 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 2030 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MV 1074 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SA 01 is an inherently dissipative polymer and can be dry blended or .. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SP 01 is an inherently dissipative polymer and can be dry blended or .. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178; ASTM D790 |
Arkema Group Pebax® MV1657 Polyether Block Amide |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
3M Dyneon™ THV 221GZ Fluoroplastic Granules 3M™ Dyneon™ Fluoroplastic Granules THV 221GZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provi.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | 50% RH; ISO 178 |
Arkema Group Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SA 01 MED is a thermoplastic elastomer made of hydrophilic flexible polyether and rigid polyamide. PEBAX® MV 1074 SA 01 MED is an inherently dissipative polyme.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ASTM D790 |
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate 3M™ Dyneon™ Fluoroplastic Agglomerate THV 221AZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate or.. |
|||
Flexural Modulus | 0.0800 - 2.34 GPa | 11.6 - 340 ksi | Average value: 1.16 GPa Grade Count:22 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Pebax® MV 2080 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 2080 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 2080 is an inherently dissipative polymer and can be dry blended or compounded w.. |
|||
Flexural Modulus | 0.0800 GPa | 11.6 ksi | ISO 178 |
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |