Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | Tangent; ASTM D790 |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP630 ABS INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD-[color]-H Nylon 66, 2% MoS2 Nylon 66, 2% Molybdenum Disulfide for Lubrication and Wear, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2 Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Polymer Resources NY66-MD2 Nylon 66, 2% MoS2 Nylon 66, 2% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM-D790 |
Ineos ABS Lustran® SAN DN79 SAN Grade Lustran® SAN DN79 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for used in compounding. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM L 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedUL File Nu.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | tangent; ASTM D790 |
Spartech PP5410 Glass Fiber Reinforced Homopolymer Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790 |
Techmer ES HiFill® PET GF15 IM 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Flexural Modulus | 3.62 GPa | 525 ksi | ASTM D790-07 |
3M Scotchkote™ 2400 Pipe Renewal Liner NSF/ANSI-61 certified polyurea formulation is 100% solids and contains no epoxy resin. It is designed to help solve a wide variety of problems common to potable water systems. It utilizes a trenchle.. |