Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Vicat Softening Point | 115 °C | 239 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Vicat Softening Point | 115 °C | 239 °F | ISO 306 |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 115 - 142 °C | 239 - 288 °F | Average value: 131 °C Grade Count:15 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Hyosung Topilene C600H PP C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Vicat Softening Point | 115 °C @Load 5.00 kg |
239 °F @Load 11.0 lb |
|
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Vicat Softening Point | 115 °C | 239 °F | VST/A/50; ISO 306 |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL N110S PPE+HIPS (Europe-Africa-Middle East) NORYL N110S is an unfilled material with a Vicat B/120 of 115 ?C according ISO 306. NORYL N110S cust spec 1977 has been listed for potable water |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti.. |
|||
Vicat Softening Point | <= 115 °C | <= 239 °F | |
Sibur Discar-E PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for profile articles of technical purpose and for sheets with following pneumatic formation of auto.. |
|||
Vicat Softening Point | 115 °C | 239 °F | A50; ISO 306 |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Vicat Softening Point | 115 °C | 239 °F | ISO 306 |
Arkema Group OREVAC® 18722 Maleic Anhydride Modified Polypropylene OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 .. |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Braskem MR 435 UV LMDPE Rotational Molding Polyethylene Applications: Water tanks; toys; automotive components. Information provided by Braskem |
|||
Vicat Softening Point | 115 °C | 239 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Vicat Softening Point | 115 °C | 239 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 5% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 115 °C | 239 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East) Blow moldable, impact modifed XENOY |
|||
Vicat Softening Point | 115 °C | 239 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |